Additives and functional resins for coatings and inks
New energy, semiconductor additives
XOANONS® Dispersant
It is used for the dispersion and viscosity reduction of nanoproportion particles such as silicon carbide, silicon nitride, boron carbide, boron nitride and conductive carbon black in water-based
Model number
XOANONS®LD 1227-45W
Materialization index
Item |
Index |
Test the method or the equipment |
criterion of detection |
Composition |
Styrene maleic acid copolymer solution |
--- |
--- |
Appearance |
Light yellow to yellow slightly muddy liquid |
--- |
--- |
Solid content |
45±3 % |
Electric drying oven |
GB/T 1725-2007 |
Density |
1.06-1.10 g/ml |
Specific gravity cup |
GB/T 6750-2007 |
Viscosity |
10-50 seconds |
Tu-4 cups |
GB/T 1723-1993 |
pH value |
4-7 |
Glass electrode method |
GB/T 9724-2007 |
Note: This indicator only represents the typical results, and is not regarded as a specification, mainly with specific COA.
Application area
Dispersion, viscosity reduction, and solid content improvement of inorganic powder materials such as nano-sized silicon carbide, silicon nitride, boron carbide, and boron nitride in water-based system
Key property
?Provide steric hindrance to improve the slurry solid content;
?Reduce the slurry settlement, flocculation and other adverse phenomena;
?Improve the storage stability of the slurry.
Incorporation
First, the dispersant XOANONS®LD 1227-45W is added to the deionized water, stir evenly. And then add the powder to disperse and ground it together according to the formula.
Suggested addition
Add amount (purchased form) is based on powder 5-10%.
Storage stability
Seal and store away from light. Unopened in the original package for 24 months. Products beyond the storage period can continue to be used after passing the inspection. The container is not fully used and unprecedented, and must be closed immediately after use.
Package
25kg (plastic drum)